245 1 0 _aElectrical and morphological properties of PP and PET conductive polymer fibers
490 0 _vSynthetic Metals, 146(2), p.167-174, 2004
520 3 _aConductive fibers were obtained using two experimental processes (melt spinning and coating process). In melt spinning process, polyaniline (PANI), polypyrrole (PPy)and graphite were used in order to obtain conductive polypropylene (PP)based fibers with specific electrical and mechanical properties. PANI was treated using dodecylbenzene sulfonic acid (DBSA)to improve the solubility and the dispersion of PANI in xylene. PANI coating on PET yarns were performed by absorption of yarns through PANI solution. The electrical resistance and morphological characteristics of conductive yarns were investigated. These yarns are supposed to be used to create smart clothing, corrosion protection or conductive fabrics for electromagnetic shielding applications.
650 1 4 _aCONDUCTIVE FIBER
650 1 4 _aPOLYANILINE (PANI)
650 1 4 _aDBSA
650 1 4 _aCOATING PROCESS
700 1 2 _aKim, B.
700 1 2 _aKoncar, V.
700 1 2 _aDevaux, E.
700 1 2 _aDufour, C.
700 1 2 _aViallier, P.
856 4 0 _uhttps://drive.google.com/file/d/1ugqc8-bkWVdhEG3N6Sj9QPN-U61Dt_qC/view?usp=drivesdk
_zPara ver el documento ingresa a Google con tu cuenta: @cicy.edu.mx
942 _2Loc
_cREF1
008 250602s9999 xx |||||s2 |||| ||und|d
999 _c42253
_d42253