| 245 | 1 | 0 | _aElectrospinning of Polycaprolactone in Dichloromethane/Dimethylformamide Solvent System |
| 490 | 0 | _vAdvanced Materials Research, 849, p.337-342, 2014 | |
| 520 | 3 | _aElectrospinning of polycaprolactone (PCL)in a mixed solvent of dichloromethane (DCM)/dimethylformamide (DMF)with 1:1 volumetic mixing ratio was studied. The effects of solution concentration (5-30 percent w/v), applied voltage (10-25 kV), solution flow rate (0.1-2.0 mL/h)and collecting distance (10, 20 cm)on fiber formation and morphology were investigated. The size of PCL fibers obtained were in the range of 10s nm-2.6 µm with either bead on string or smooth fiber morphology. In this study, the solution concentration strongly affected fiber size exponentially. The fiber size also increased with an increase in solution flow rate. The applied voltage and the collecting distance have no or minimal effect on PCL fiber size. | |
| 650 | 1 | 4 | _aPOLYCAPROLACTONE |
| 650 | 1 | 4 | _aELECTROSPINNING |
| 650 | 1 | 4 | _aDICHLOROMETHANE |
| 650 | 1 | 4 | _aDIMETHYLFORMAMIDE |
| 700 | 1 | 2 | _aNarissara Kulpreechanan |
| 700 | 1 | 2 | _aTanom Bunaprasert |
| 700 | 1 | 2 | _aRatthapol Rangkupan |
| 856 | 4 | 0 |
_uhttps://drive.google.com/file/d/1DkJukqnUpFQmTsxpSwBvzcrYiGWEpZ4a/view?usp=drivesdk _zPara ver el documento ingresa a Google con tu cuenta: @cicy.edu.mx |
| 942 |
_2Loc _cREF1 |
||
| 008 | 250602s9999 xx |||||s2 |||| ||und|d | ||
| 999 |
_c49186 _d49186 |
||