245 1 0 _aDependence of the gas permeability of some polyimide isomers on their intrasegmental mobility
490 0 _vJournal of Membrane Science, 77(1), p.41-48, 1993
520 3 _aThe polyimide PMDA-4,4'-ODA has a higher permeability and a lower selectivity toward H2, CO2, CH4, O2, and N2 than its isomer PMDA-3,3'-ODA. The differences in the gas permeability and selectivity are attributed to differences in the intrasegmental (rotational)mobility of PMDA-4,4'-ODA (the para-isomer)and of PMDA-3,3'-ODA (the meta-isomer). The phenyl rings in the para-isomer can rotate around their principal axis whereas such a rotation is not possible in the meta-isomer. This hypothesis is supported by dynamic mechanical analyses as well as by measurements of the CO2 diffusivity in the two isomers. Computer simulations indicate that rotation of the phenyl ring in the para-isomer is hindered by two larger rotational energy barriers of 4.0 and 2.4 kcal/mole, and two smaller ones of 1.3 kcal/mole. © 1993.
650 1 4 _aCARBON DIOXIDE
650 1 4 _aCOMPUTER SIMULATION
650 1 4 _aDIFFUSION
650 1 4 _aHYDROGEN
650 1 4 _aMECHANICAL PERMEABILITY
650 1 4 _aMETHANE
650 1 4 _aMOLECULAR STRUCTURE
650 1 4 _aNITROGEN
650 1 4 _aOXYGEN
650 1 4 _aPOLYIMIDES
700 1 2 _aMi, Y.
700 1 2 _aStern, S.A.
700 1 2 _aTrohalaki, S.
856 4 0 _uhttps://drive.google.com/file/d/17ma_m0OSCBhVtTh5hIfsbRfyB2IjX34t/view?usp=drivesdk
_zPara ver el documento ingresa a Google con tu cuenta: @cicy.edu.mx
942 _2Loc
_cREF1
008 250602s9999 xx |||||s2 |||| ||und|d
999 _c50001
_d50001