245 1 0 _aBehaviour of rare earth sesquioxides exposed to atmospheric carbon dioxide and water
490 0 _vReactivity of Solids, 4(1-2,), p.23-40, 1987
520 3 _aThe behaviour of the rare earth sesquioxides, when exposed to atmospheric water and carbon dioxide under ordinary conditions of temperature and pressure, is reviewed. Data corresponding to eleven samples from seven different oxides systematically investigated by X-ray diffraction (XRD), IR spectroscopy, thermogravimetry (TG)and temperature-programmed decomposition (TPD), are reported. The BET surface areas of all these samples are also given. In accordance with the results summarized, upon exposure to air, the lanthanide sesquioxides all become hydrated and carbonated in bulk. However, the rate and intensity of these processes, as well as the nature of the resulting phases, are not the same for the whole group of oxides. Furthermore, the characterization carried out on the oxides aged in air suggests that throughout the lanthanide series at least three types of behaviour can be distinguished. In some cases, the behaviour has been found to depend on the origin of the samples, which prevents the generalization of definite sequences of reactivity for the whole series of oxides. Also, the use of a single technique, particularly XRD, does not allow one to establish the nature of the aged phases, or even to determine whether or not alterations in the bulk of the starting oxides have occurred. © 1987.
650 1 4 _aENVIRONMENTAL TESTING
650 1 4 _aOXIDES - CHEMICAL REACTIONS
650 1 4 _aSPECTROSCOPY, INFRARED
650 1 4 _aTHERMOANALYSIS
700 1 2 _aBernal, S.
700 1 2 _aBotana, F.J.
700 1 2 _aGarcía, R.
700 1 2 _aRodríguez-Izquierdo, J.M.
856 4 0 _uhttps://drive.google.com/file/d/1pzYgcMM_iV-4hIr6rBjogwLbw33uC3iz/view?usp=drivesdk
_zPara ver el documento ingresa a Google con tu cuenta: @cicy.edu.mx
942 _2Loc
_cREF1
008 250602s9999 xx |||||s2 |||| ||und|d
999 _c50238
_d50238