Mucoadhesive chitosan-coated liposomes: characteristics and stability

Tipo de material: TextoTextoSeries ; Journal of Microencapsulation, 18(1), p.3-12, 2001Trabajos contenidos:
  • Filipovic-Grcic, J
  • Skalko-Basnet, N
  • Jalsenjak, I
Tema(s): Recursos en línea: Resumen: Lecithin liposomes, empty or containing FITC-dextran, were prepared by the ethanol injection method. Three diå erent types of chitosans with diå erent molecular weight and degrees of deacetylation were used (Seacure 113, 210 and 311). Chitosan coating was carried out by mixing the liposomal suspension with the chitosan solution followed by incubation. The size of liposomes was measured before and after polymer coating by an image analysis technique. The mean diameter of liposomes containing FITC-dextran was in the size range 250± 280nm, whereas the size after coating was 300± 330 nm, regardless of chitosan type. All chitosan-coated liposomes were of spherical shape and no morphological diå erences between uncoated and coated liposomes were observed. Liposomes with FITC-dextran, originally entrapping 50
Tags from this library: No tags from this library for this title. Log in to add tags.
Star ratings
    Average rating: 0.0 (0 votes)
Holdings
Item type Current library Collection Call number Status Date due Barcode
Documentos solicitados Documentos solicitados CICY Documento préstamo interbibliotecario Ref1 B-10979 (Browse shelf(Opens below)) Available

Lecithin liposomes, empty or containing FITC-dextran, were prepared by the ethanol injection method. Three diå erent types of chitosans with diå erent molecular weight and degrees of deacetylation were used (Seacure 113, 210 and 311). Chitosan coating was carried out by mixing the liposomal suspension with the chitosan solution followed by incubation. The size of liposomes was measured before and after polymer coating by an image analysis technique. The mean diameter of liposomes containing FITC-dextran was in the size range 250± 280nm, whereas the size after coating was 300± 330 nm, regardless of chitosan type. All chitosan-coated liposomes were of spherical shape and no morphological diå erences between uncoated and coated liposomes were observed. Liposomes with FITC-dextran, originally entrapping 50